為(wei)提升紙盒(he)的(de)檔次與美(mei)觀(guan)度,通(tong)常會對紙盒(he)表層進行上光、覆(fu)(fu)膜(mo)等處(chu)理。然而(er),這些處(chu)理方式卻給紙盒(he)熱熔(rong)膠的(de)粘(zhan)結(jie)帶來了極大(da)挑戰。倘若遇到(dao)覆(fu)(fu)膜(mo)后的(de)紙(zhi)盒用(yong)熱(re)熔膠粘不牢的情況,該(gai)如何應對呢(ni)?
紙(zhi)(zhi)盒(he)熱熔(rong)膠(jiao)難以(yi)粘(zhan)住覆膜后(hou)的紙(zhi)(zhi)盒(he)。若(ruo)不想更換現(xian)有(you)的紙(zhi)(zhi)盒(he)用熱熔(rong)膠(jiao),有(you)兩(liang)種可行(xing)(xing)之法。其一(yi),在需(xu)要(yao)用熱熔(rong)膠(jiao)粘(zhan)合的部位,不進(jin)行(xing)(xing)覆膜和上(shang)光處理,為熱熔(rong)膠(jiao)的粘(zhan)結預留(liu)位置;其二,破(po)壞(huai)紙(zhi)(zhi)盒(he)粘(zhan)合處的材(cai)質(zhi)。覆膜后(hou)的材(cai)質(zhi)不利于(yu)熱熔(rong)膠(jiao)滲透(tou)(tou),而對粘(zhan)合處材(cai)質(zhi)進(jin)行(xing)(xing)破(po)壞(huai)有(you)助于(yu)熱熔(rong)膠(jiao)滲透(tou)(tou),從而增強粘(zhan)著效果。邦林的紙(zhi)(zhi)盒(he)用(yong)熱(re)(re)熔(rong)(rong)膠(jiao)已(yi)持續十年為(wei)致力于(yu)美化環境(jing)的紙(zhi)(zhi)盒(he)客戶提供穩定(ding)(ding)的解(jie)決方案。使(shi)用(yong)邦林紙(zhi)(zhi)盒(he)用(yong)熱(re)(re)熔(rong)(rong)膠(jiao),實(shi)現了牢固的粘結(jie)、便(bian)利的施工以及優越的高(gao)低溫(wen)性(xing)能(neng),為(wei)紙(zhi)(zhi)盒(he)生產商提供了穩定(ding)(ding)且高(gao)附(fu)加值的供應保障。